FOUNDRY ALLOYS
INOCULANTS
50% Ferrofilison
Foundry Grade
75% Ferrofilison
Foundry Grade
Inocast 100
(Inolate 100)*
Si
Al
Ca
47-51%
.60-1.25%
.50-1.50%
Si
Al
Ca
74-79%
.80-1.50%
.50-1.50%
Si
Al
Ca
62-69%
3.2-4.5%
.50-1.50%
Win-4*
FeSila*
Grafidin
(Inolate 10)*
Si
Al
Ca
Ba
Bi
La

62-68%
.7-1.0%
.1.5-3.5%
0.1-0.5%
.10-50%
.50-1.5%

Si
Al
Ca
La



45-50%
1.25% Max
1.5-2.5%
1.8-2.2%
Also Available in 65% Si


Si
Al
Ca
Mn
Ba


60-67%
.80-1.7%
1.7-3.2%
7-11%
3.7-5.7%
LMC*
(Inolate 196)*
HW-5
Inobar
(Inolate 20)*
Si
Al
Ca
Ba
63-70%
.50-1.1%
1.2-2.1%
.50-1.2%
Si
Al
Ca
Ba
70-77%
.80-1.50%
.80-1.50%
1.5-2.5%
Si
Al
Ca
Ba
60-67%
.80-1.7%
.40-1.7%
7-11%
Inostrong 50*
Inostrong
(Inolate 30)*
Spherix
(Inolate 40)*
Si
Al
Ca
Sr
46-50%
.50% Max
.10% Max
.60-1.10%
Si
Al
Ca
Sr
73-80%
.5% Max
.1% Max
.60-1.1%
Si
Al
Ca
Bi
TRE
70-75%
.70-1.4%
1-2%
.80-1.3%
.40-.70%
Incocast 125
(Inolate 190)*
Zircograf
(Inolate 50)*
ZL-80
(Inolate 60)*
Si
Al
Ca
Mn
Zr
Ba
62-69%
.55-1.3%
.60-1.9%
2.8-4.5%
3-5%
.60% Max
Si
Al
Ca
Mn
Zr
62-68%
.70-1.50%
.50-2.0%
5-6.7%
5-6.7%
Si
Al
Ca
Zr
72-80%
1-1.8%
1.5-3.5%
1.2-2.0%
Moldinco 65*
In Mold Inserts
Moldinco 75*
In Mold Inserts
HW Cubes
Si
Al
Ca
Mn
Ba
64-67%
.80-1.1%
.80-1.2%
.25% Max
.15% Max
Si
Al
Ca
Mn
Ba
75-80%
2.5-3.5%
.20-.60%
.25% Max
.15% Max
Si
Al
Ca

74-79%
.80-1.50%
.70-1.50%

MOLDINOC 65 available in 25, 50, 70, 90 or 180 gram sizes. MOLDINOC 75 available in 20, 40, 60, 80 or 150 gram sizes. Available in 20-30 gram, 30-40 gram, 50-60 gram and other sizes in 10 gram increments.
MAGNESIUM FERROSILICON TREATMENT ALLOYS
Rare Earth Free Grades %Mg %Si %Ca %Al
HW-Mag 3 2.90-3.40 44.0-48.0 .80-1.35 1.25 Max
HW-Mag 5 5.50-6.50 44.0-48.0 .80-1.35 1.25 Max  
MAG 910* .84-9.60 42.0-50.0 .80-1.60 .80 Max
Carium Bearing Grades %Mg %Si %Ca %Al %Ce
HW-Mag 5L 5.50-6.50 44.0-48.0 .80-1.35 1.25 Max .30-.40
HW-Mag 5M 5.50-6.50 44.0-48.0 .80-1.35 1.25 Max .45-.70
HW-Mag 5M-HP 5.50-6.50 44.0-48.0 .30 Max .30 Max .45-.70
HW-Mag 5H 5.50-6.50 44.0-48.0 .80-1.35 1.25 Max .90-1.25
Blended Rare Earth
Grades
%Mg %Si %Ca %Al Total Rare
Earth
HW-Mag 3LA 3.00-3.80 44.0-48.0 .80-1.35 1.25 Max 1.50-2.20
HW-Mag 3LAFT 3.00-3.80 44.0-48.0 .80-1.35 1.25 Max 1.30-1.80
HW-Mag 5LA 5.50-6.50 44.0-48.0 .80-1.35 1.25 Max .50-.85
HW-Mag 5LB 5.50-6.50 44.0-48.0 .80-1.35 1.25 Max .75-1.10
HW-Mag 5LC 5.50-6.50 44.0-48.0 .80-1.35 1.25 Max 1.25-1.75
Calcium
Modified Grades
%Mg %Si %Ca %Al Total Rare Earth
HW-Mag 4LBHIC 4.5-5.5 44.0-48.0 1.80-2.25 1.25 Max TRE .50-.85
HW-Mag 5LBHIC 5.5-6.5 44.0-48.0 1.80-2.25 1.25 Max TRE .50-.85
In Mold Treatment %Mg %Si %Ca %Al Total Rare Earth
SIMAF* 5.0-6.5 42.0-50.0 .20-.60 .60-1.40 TRE .25-.40

* Trademark of Ferroatlantica-PEM Division


Inoculants are available in standard ladle and injection sizes.
Inolate is a designation for late inoculation size.

Magnesium Ferrosilicon treatment alloys are available in standard industry sizes
including stream treatment applications.
           
           
< - - - - Back - - - - -